(Cancelled) Analysis of Casting Defects 3 credits
The course covers the most common casting defects, how they are identified and characterized, causes of their formations, the basic mechanisms and measures to minimize or eliminate their occurrence.
For more information see https:ju.se/studera/valj-utbildning/kompetensutveckling---uppdragsutbildning/tekniska-hogskolan/gjutfelsanalys-analysis-of-casting-defects.html
Course Contents
The course covers the most common casting defects, how they are identified and characterized, causes of their formations, the basic mechanisms and measures to minimize or eliminate their occurrence.
The course includes the following elements:
- Identification of different types of casting defects
- Defect formation - Causes and mechanisms
- Prediction of defects using simulation tools
- Practical examinations
- Root cause analysis
- Case studies
Prerequisites
Passed courses at least 90 credits within the major subject Mechanical Engineering, 15 credits Mathematics, and completed course in Solidification Processing, 3 credits and proof of English proficiency is required (or the equivalent).
Level of Education: Second cycle
Coursecode/Ladok code: TGAS22
The course is conducted at: School of Engineering
| Label | Value |
|---|---|
| Type of course | Programme instance course |
| Study type | Online Distance Learning |
| Number of required meetings | 0 |
| Semester | Autumn 2025 |
| Study period |
week 36 - week 43
|
| Rate of study | 100% |
| Language | English |
| Location | Web-based |
| Time | Mixed-time |
| Tuition fees do NOT apply for EU/EEA citizens or exchange students | 8550 SEK |
| Syllabus (PDF) | |
| Application code | HJ-T3269 |